MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Silon Taborex TA 2120 HD Catalyst Masterbatch
Categories: Other Engineering Material; Catalyst/Initiator

Material Notes: Masterbatch for the use with SILON Silane crosslinkable PE-Xb Compounds TA 1104 HD, TA 1105 HD, TA 1116 HD. TA 2120 HD contains the cross-linking catalyst to complete together with the above-mentioned graft a Sioplas System. In addition it carries a part of the long term stabilising system for the finished product.

Information provided by Silon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.540 g/cc
Density 0.960 g/cc
Volatiles >= 0.050 %
Melt Flow 8.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
Storage Temperature <= 25.0 °C
 
Descriptive Properties
ColorWhite, translucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silon Taborex TA 1108 HD Chemically-Crosslinkable HDPE Compound
Syensqo (Solvay Specialty Polymers) Catalyst Masterbatch CT/7-LR UV Polyolefin
Silon TA 2323 HD White Catalyst Masterbatch

PSILON09 / 83547

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.