MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Aronkasei TF-A90NT SEBS
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Characteristics:
  • High rubber elasticity
  • Excellent grip performance
  • Excellent in resistance to weather and ozone
  • Over molding and co-extrusion molding with olefin resins are possible
  • Good moldability (No flow mark)
Examples of Use:
Automotive parts : Lamp accessories, Grommet, Trim panel, Edge, Door switch cover, etc
Electric equipment parts : Vibration insulating rubber, Water-proof packing, Power tool grip, Rubber leg, Printer roller, etc
Others : Cutting blade, Tool grip, Golf club grip, Furniture, Building parts, etc

Information provided by ARONKASEI CO.,LTD Elastomer Dept.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.01 g/ccJIS K 7112
Linear Mold Shrinkage 0.0080 - 0.016 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 87JIS K 6253
Tensile Strength at Break 16.7 MPaJIS K 6251
Elongation at Break 800 %JIS K 6251
Resilience 36[%]; JIS K 6252
Tear Strength 51.0 kN/mJIS K 6252
Compression Set 34 %
@Temperature 23.0 °C,
Time 86400 sec
JIS K 6262
 53 %
@Temperature 70.0 °C,
Time 86400 sec
JIS K 6262
 64 %
@Temperature 100 °C,
Time 86400 sec
JIS K 6262
 
Thermal PropertiesOriginal ValueComments
Melting Point 156 °CJIS K 7121
Softening Point 147 °C
Brittleness Temperature <= -60.0 °CJIS K 6261
 
Descriptive Properties
ColorBlack / Milky-White (Natural)
Molding MethodInjection / Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PJARON006 / 293918

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.