MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Nucrel® 0902HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
Categories: Polymer; Film; Thermoplastic; Ethylene Methyl Acrylate; Ethylene-Methyl Acrylate Copolymer, Film Grade

Material Notes: 9 wt% Methacrylic Acid.

Nucrel® 0902HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins.

Features/Benefits vs. Nucrel® 0403HC: Better adhesion to coextruded nylon for improved structure reliability and barrier integrity. Higher film strength for improved structure reliability and product protection. Lower seal initiation temperature for higher speed packaging. Better hot tack, sealability through contamination, and heat seal strength for stronger, more reliable heat seals. Better film optics for better package appearance and/or better product visibility.

Typical Applications: Meat, poultry, seafood, and cheese packaging; Cereal liners; Medical/pharmaceutical packaging; Powdered/granular food and non-food pouches; Carded display/skin packaging films; Edible oil, motor oil, and other liquid product pouches; Snack structures; Coextrusions with nylon or in other film structures as a heat seal or tie layer.

Information provided by DuPont Packaging Polymers.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 1.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 450 %450 %50 µm (2 mil) film; ASTM D882
Film Elongation at Break, TD 450 %450 %50 µm (2 mil) film; ASTM D882
Secant Modulus, MD 0.159 GPa23.1 ksi50 µm (2 mil) film; ASTM D882
Secant Modulus, TD 0.131 GPa19.0 ksi50 µm (2 mil) film; ASTM D882
Impact 2929J/mm Spencer Impact; ASTM D3420
Elmendorf Tear Strength, MD 4.72 g/micron120 g/mil50 µm (2 mil) film; ASTM D1922
Elmendorf Tear Strength, TD 5.12 g/micron130 g/mil50 µm (2 mil) film; ASTM D1922
Dart Drop 7.90 g/micron201 g/milASTM D1709B
Hot Tack Strength 1800 g/25 mm1800 g/inseal bar 105°C; Packforsk method.
Film Tensile Strength at Break, MD 33.1 MPa4800 psi50 µm (2 mil) film; ASTM D882
Film Tensile Strength at Break, TD 36.5 MPa5290 psi50 µm (2 mil) film; ASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 78.0 °C172 °FFreezing Point via DSC/ASTM D3418
 103 °C217 °FUpon Melting via DSC/ASTM D3418
Vicat Softening Point 81.0 °C178 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 2.5 %2.5 %ASTM D1003
Gloss 65 %65 %20°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 191 °C376 °FTypical Die Temp.
Melt Temperature 190 - 218 °C374 - 424 °Fblown film equipment

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Nucrel® 1202HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
Dow Nucrel® 0411HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
Dow Nucrel® 960 Ethylene-Methacrylic Acid Copolymer Resin
Dow Nucrel® 925 Ethylene-Methacrylic Acid Copolymer Resin
Dow Nucrel® 0903HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film

PDUPJ5 / 33639

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.