MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Formed and Deep Draw Quality
Categories: Metal; Electronic/Magnetic Alloy; Superalloy; Iron Base

Material Notes: High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC circuits in which the frequency is less than 400 cycles per second. Following a low temperature hydrogen anneal at 1300/1400°F (704/760°C), alloy 49 exhibits constant permeability characteristics. Its initial permeability is approximately 500 Gauss. High Permeability "49" alloy resists weather and moisture corrosion to a moderate extent.

High permeability "49" alloy has been used in laminated cores for instrument transformers, magnetic shields and cores for certain electronic and communications devices in which extremely high permeability at low magnetizing forces greatly increases the efficiency and effectiveness of the equipment. Because of its high permeability, it has also been used in solenoid cores in light, sensitive relays that must operate and respond to weak currents that induce low magnetizing forces.

If components are to machined in volume from bar stock, High Permeability "49"-FM, a free-machining grade, is recommended. The standard grade , High Permeability "49" alloy, machines somewhat like the austenitic stainless alloys. It develops gummy chips but does not work harden as rapidly as the stainless alloys. Sulfur-bearing cutting compounds are highly detrimental to the final magnetic properties. Animal lard oil should be used in drilling and machining operations which must be performed at low speeds. Work hardened bars offer the best machining characteristics. Parts should be degreased and cleaned as soon as possible.

Information provided by High Temp Metals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 8.18 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 68
Tensile Strength, Ultimate 80000 psi
Elongation at Break 32 %
Modulus of Elasticity 166 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000480 ohm-cmTemperature coefficient = 0.0036/°C (-17.8 to 499°C)
Magnetic Permeability 8000Initial; B100; per ASTM A596, 0.025 - 0.125 in. thickness; heat treatment unknown
 12000Initial; B100; per ASTM A596, 0.014 in. thickness; heat treatment unknown
 90000Maximum; per ASTM A596, 0.025 - 0.125 in. thickness; heat treatment unknown
 150000Maximum; per ASTM A596, 0.014 in. thickness; heat treatment unknown
Magnetic Coercive Force, Hc 0.040 - 0.070 Oefrom 10,000 Gauss; per ASTM A596, 0.014 in. thickness; heat treatment unknown
 0.040 - 0.070 Oefrom 10,000 Gauss; per ASTM A596, 0.025 - 0.125 in. thickness; heat treatment unknown
Magnetic Saturation Flux Density, Bmax 15000 GaussH-100 Oersted; per ASTM A596, 0.025 - 0.125 in. thickness; after hydrogen annealing
 15000 GaussH-100 Oersted; per ASTM A596, 0.014 in. thickness; after hydrogen annealing
Magnetic Remanence, Br 9000 Gaussper ASTM A596, 0.025 - 0.125 in. thickness; heat treatment unknown
 9000 Gaussper ASTM A596, 0.014 in. thickness; heat treatment unknown
Curie Temperature 450 - 500 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.60 µin/in-°F
@Temperature 25.0 - 204 °C
Specific Heat Capacity 0.120 BTU/lb-°F
Thermal Conductivity 13.0 W/m-K
Melting Point 2600 °F
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.020 %
Iron, Fe >= 51 %As Balance
Manganese, Mn <= 0.50 %
Nickel, Ni <= 48 %
Silicon, Si <= 0.35 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Cold Drawn
303 Stainless Steel, annealed
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Hydrogen Annealed at 2150°F (1177°C)
303 Stainless Steel, Cold worked wire
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, After Process Annealed at 1600°F (871°C)

NHIGH004 / 17307

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.