MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay GEROPON® HW 15 Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description Ethoxylated carboxylates Emulsifier for metal working formulations with excellent dispersing power for calcium soaps. Avoids the formation of insoluble precipitates, and consequently improves the lubricant stability in hard water. Suitable for all water based Metal Working fluids ranging from synthetic and semi-synthetic lubricants to soluble oils.

Identification: ALCOHOL ETHO-CARBOXYLATED ACID FORM

Solubility Soluble in water. Dispersible in oils

Available in: Asia Pacific, Europe, Latin America and North America

Applications: Anionic emulsifier for Metal Working Fluids and lime soap dispersant. GEROPON HW 15 can provide excellent hard water resistance to aqueous Metal working Fluids.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³
pH 1.6 - 2.81.6 - 2.810% aq. Sol.; 540MA3C1E
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 69 - 7969 - 79[mg KOH/g]; 540MA3C21
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 100 °C>= 212 °F
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 6.0<= 6.0540MA3C1D
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 6.0 - 10 %6.0 - 10 %540MA3C1C
 
Descriptive Properties
AppearanceYellow liquid to gel
CompositionActives (100-%water-%NaCl)>89%
 NaCl<1.5%, 540MA3C10
Ionic ChargeAnionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay RHODAFAC® PA32 Surfactant
Solvay RHODAFAC® RS-610 Surfactant
Solvay GEROPON® HW 15 N Surfactant
Solvay RHODAQUAT® M-242B/99 Surfactant
Solvay GEROPON® DOS/PG Surfactant

WRHOD123 / 137354

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.