MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Bormed™ LE6607-PH LDPE for Pharmaceutical Blow Molding
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Blow Molding Grade

Material Notes: Bormed LE6607-PH is a LD-polyethylene produced in a high pressure process intended for blow molding of sot and flexible packages for pharmaceutical products.

Bormed LE6607-PH can be used in "blow-fill and seal" machines for the production of ampoules and bottles. The product can also be used for pharmaceutical products manufactured with other conversion techniques such as injection molding and film blowing. LE6607-PH will withstand heating up to 110°C and therefore units made from this product may be steam treated to max 110°C.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.927 g/ccISO 1183
Melt Flow 0.30 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 52ISO 868
Tensile Strength, Yield 1740 psiAt 50 mm/min; ISO 527-2
Elongation at Break 700 %At 5 mm/min; ISO 527-2
Flexural Modulus 0.320 GPaAt 2 mm/min; ISO 178
 
Processing PropertiesOriginal ValueComments
Melt Temperature 165 - 200 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Bormed™ LE6601-PH LDPE for Pharmaceutical Blow Molding
BASF Novolen® 1102 H Polypropylene
Amco PRIMATOP LDPE 023919 Blow Molding Polyethylene
Borealis Bormed™ LE6609-PH LDPE for Pharmaceutical Blow Molding
Borealis FA6224 Low Density Polyethylene

PBOREA078 / 27385

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.