MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Eastman Amphora™ FL6000 Flexible 3D Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Amphora™ Flex 3D polymer FL6000, a flexible material engineered for extrusion-based additive manufacturing processes. Amphora Flex FL6000 is a polymer that can be used with standard 3D printers, eliminating the need to switch to specialized flex extruders. Because of exceptional layer-to-layer adhesion and melt strength, it prints at a faster speed than other elastomeric materials, saving time. Amphora Flex FL6000 is an engineering-grade material that demonstrates superior durability and toughness, enabling designers to quickly create truly functional parts that can withstand the rigors of everyday use. Amphora Flex FL6000 is highly useful for applications that demand both the durability of an engineering-grade polymer and the comfort and utility of a flexible material. With a Shore A hardness level of 95, outstanding chemical resistance, and a temperature resistance that allows steam sterilization, users may find it useful for additive manufacturing of prosthetics, orthotics, automotive parts, apparel, tooling, or a variety of consumer products.

Application/Uses:

  • Production of 3D Printing filaments
Key Attributes:
  • Dimensional stability
  • Enhanced aesthetics
  • Excellent Temperature Resistance
  • Excellent toughness
  • Extended Processing Window
  • Low odor
  • Property retention in 3D applications
  • Steam Sterilizable
  • Styrene-free
  • Workability

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 95ASTM D2240
Hardness, Shore D 55ASTM D2240
Tensile Strength at Break 22.0 MPaASTM D638
Tensile Strength, Yield 14.0 MPaASTM D638
Elongation at Break 400 %ASTM D638
Elongation at Yield 38 %ASTM D638
Flexural Modulus 150 MPaASTM D790
Izod Impact, Notched 0.400 J/cm
@Temperature -40.0 °C
ASTM D256
Tear Strength Test 350N; ASTM D1004
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 170 °CASTM D1525
Brittleness Temperature <= -70.0 °CASTM D746
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 - 260 °C
 
Descriptive Properties
Processing - CoolingAs needed up to 50%
Processing - Heated Bed 80°C
Processing - InfillAs needed up to 100%
Processing - Layer Height0.1 or 0.2 mm
Processing - Minimal Layer Time5 s
Processing - Perimeterapprox. 1 mm
Processing - Speed30-50 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese D Antistat 907 kg-51007157 91-93% Paraformaldehyde
Celanese 50000767 91-93% Paraformaldehyde
Special Metals Electroformed Nickel Foil, As-Electroformed
Special Metals Electroformed Nickel, 13 Micron (0.5 mil) Foil, Electroformed and Annealed
Special Metals Electroformed Nickel, 200 Micron (8 mil) Foil, Electroformed and Annealed

PE8930g / 217531

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.