MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon
Categories: Ceramic; Carbide; Ceramic Matrix Composite

Material Notes: Engineered ceramic composite structure.

Reinforcing Fiber Flexibility: S400 - Carbon
Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiC
Physical Attributes: Dense Matrix (<5%), High Temperature Capability, Good Matrix Dominated Properties and Wear Resistance

Typical Applications: Commercial Aviation Exhaust, Military Aircraft Propulsion Exhaust, Industrial

Information from COI Ceramics, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 262 MPa
@Treatment Temp. 20.0 °C
 300 MPa
@Treatment Temp. 1000 °C
Tensile Strength, Yield 13.0 ksi
@Strain 0.08 %,
Temperature 1000 °C
 14.0 ksi
@Strain 0.09 %,
Temperature 20.0 °C
Tensile Stress at Strain 7.11 ksi
@Strain 0.05 %,
Temperature 1204 °C
 7.25 ksi
@Strain 0.05 %,
Temperature 20.0 °C
 8.70 ksi
@Strain 0.05 %,
Temperature 982 °C
 13.1 ksi
@Strain 0.1 %,
Temperature 1204 °C
 13.8 ksi
@Strain 0.1 %,
Temperature 982 °C
 15.2 ksi
@Strain 0.1 %,
Temperature 20.0 °C
 23.2 ksi
@Strain 0.3 %,
Temperature 1204 °C
 24.7 ksi
@Strain 0.3 %,
Temperature 982 °C
 26.8 ksi
@Strain 0.3 %,
Temperature 20.0 °C
 32.6 ksi
@Strain 0.5 %,
Temperature 1204 °C
 34.8 ksi
@Strain 0.5 %,
Temperature 982 °C
 37.7 ksi
@Strain 0.5 %,
Temperature 20.0 °C
Elongation at Break 0.50 %
@Temperature 20.0 °C
 0.70 %
@Temperature 1000 °C
Elongation at Yield 0.08 %
@Temperature 1000 °C
Proportional Limit
 0.09 %
@Temperature 20 °C
Proportional Limit
Tensile Modulus 90.0 GPa
@Temperature 1000 °C
 96.0 GPa
@Temperature 20.0 °C
Flexural Strength 55.0 ksi
@Temperature 20.0 °C
 60.0 ksi
@Temperature 1000 °C
Compressive Strength 434 MPa
@Temperature 20.0 °C
Shear Strength 24.0 MPa
@Temperature 1000 °C
 38.0 MPa
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.80 W/m-K
@Temperature 100 °C
Thru-thickness
 1.80 W/m-K
@Temperature 200 °C
Thru-thickness
 1.80 W/m-K
@Temperature 300 °C
Thru-thickness
 1.80 W/m-K
@Temperature 500 °C
Thru-thickness
 1.85 W/m-K
@Temperature 700 °C
Thru-thickness
 1.85 W/m-K
@Temperature 500 °C
Fill direction
 1.85 W/m-K
@Temperature 500 °C
Warp direction
 1.90 W/m-K
@Temperature 300 °C
Warp direction
 1.90 W/m-K
@Temperature 900 °C
Thru-thickness
 1.90 W/m-K
@Temperature 300 °C
Fill direction
 1.95 W/m-K
@Temperature 200 °C
Warp direction
 1.95 W/m-K
@Temperature 200 °C
Fill direction
 1.95 W/m-K
@Temperature 1000 °C
Thru-thickness
 1.95 W/m-K
@Temperature 700 °C
Fill direction
 1.95 W/m-K
@Temperature 700 °C
Warp direction
 2.10 W/m-K
@Temperature 1000 °C
Warp direction
 2.10 W/m-K
@Temperature 1000 °C
Fill direction
 2.10 W/m-K
@Temperature 1200 °C
Thru-thickness
 2.15 W/m-K
@Temperature 100 °C
Warp direction
 2.15 W/m-K
@Temperature 100 °C
Fill direction
 2.15 W/m-K
@Temperature 900 °C
Fill direction
 2.15 W/m-K
@Temperature 900 °C
Warp direction
 2.40 W/m-K
@Temperature 1200 °C
Warp direction
 2.40 W/m-K
@Temperature 1200 °C
Fill direction

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
COI Ceramics Sylramic™ S400 Silicon Carbide Ceramic Matrix Composite, Carbon
Mid-Mountain Materials SILTEX® 36 Amorphous Silica Textile
COI Ceramics Nextel™ AS-N312 Oxide Ceramic Matrix Composite, Aluminosilicate
Schunk SiC30 Silicon Carbide/Graphite Composite
COI Ceramics Nextel™ AS-N720 Oxide Ceramic Matrix Composite, Aluminosilicate

CCOIC008 / 122048

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.