MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Industeel URANUS® 45N+ 22% Cr Austenitic-Ferritic Duplex Stainless Steel
Categories: Metal; Ferrous Metal; Duplex; Stainless Steel; T S30000 Series Stainless Steel

Material Notes: Description: URANUS® 45N+ (UR 45N+) is a nitrogen alloyed austenitic-ferritic Duplex stainless steel (22.05), with a minimum PREN value guaranteed of 36 due to over-alloying in Molybdenum and Chromium. This alloy presents higher mechanical and corrosion resistance properties than duplex 22 Cr stainless steels. Its yield strength is about twice that of standard austenitic grades and well in excess of that of nitrogen alloyed austenitics. Operation temperature of UR 45 N+ is generally limited from -50°C to 280°C (- 58°F to 536°F). Lower temperature used particularly for welded structures may also be considered, but needs technical background.

Information provided by manufacturer.

Key Words: EURONORM 1.4462 - X2 Cr Ni Mo N 22.5.3, AFNOR Z3 CND 22.05.AZ, WERKSTOFF Nr 1.4462, UNS S31803, UNS S32205
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate >= 720 MPa>= 104000 psi
Tensile Strength, Yield  >= 510 MPa
@Strain 0.2 %
>= 74000 psi
@Strain 0.2 %
 >= 540 MPa
@Strain 1 %
>= 78300 psi
@Strain 1 %
Elongation at Break >= 25 %>= 25 %
Modulus of Elasticity 200 GPa29000 ksi
Poissons Ratio 0.3330.333Calculated
Shear Modulus 75.0 GPa
@Temperature 20.0 °C
10900 ksi
@Temperature 68.0 °F
Charpy Impact >= 90.0 J>= 66.4 ft-lb
 120 J88.5 ft-lbTypical
 >= 75.0 J
@Temperature -50.0 °C
>= 55.3 ft-lb
@Temperature -58.0 °F
 90.0 J
@Temperature -50.0 °C
66.4 ft-lb
@Temperature -58.0 °F
Typical
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000800 ohm-cm
@Temperature 20.0 °C
0.0000800 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.0 µm/m-°C
@Temperature 20.0 - 100 °C
6.67 µin/in-°F
@Temperature 68.0 - 212 °F
 12.5 µm/m-°C
@Temperature 20.0 - 200 °C
6.94 µin/in-°F
@Temperature 68.0 - 392 °F
 13.0 µm/m-°C
@Temperature 20.0 - 300 °C
7.22 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.450 J/g-°C
@Temperature 20.0 °C
0.108 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity 17.0 W/m-K
@Temperature 20.0 °C
118 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.020 %0.020 %
Chromium, Cr 22.6 %22.6 %
Iron, Fe 67.799 %67.799 %As remainder
Molybdenum, Mo 3.4 %3.4 %
Nickel, Ni 6.0 %6.0 %
Nitrogen, N 0.18 %0.18 %
Sulfur, S 0.0010 %0.0010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Industeel URANUS® 45N 22Cr 3Mo Duplex Stainless Steel with PREN = 33 or 34
Outokumpu 2205 Duplex Stainless Steel
Carlson 2205 (UNS S31803) Duplex Stainless Steel
ATI Allegheny Ludlum AL 2205™ Duplex Stainless Steel, Plate > 0.1875" Duplex Stainless Steel, UNS S31803
MetalTek MTEK 2205 Cast UNS J92205 Duplex Stainless Steel

NINDUST14 / 17552

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.