MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

(Viewing data as-entered. Click here to return)
Saint-Gobain Meldin® 3000G Bearing  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes: General Notes on Meldin 3000/5000 Series Bearing Products:
Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.
Specific Notes on Meldin®3000G Bearing
Meldin® 3000G should be used when the combination of high strength and electrical insulation is required. Components made from this material exhibit superior properties in tensile, flex and resistance to deformation under load.

Applications include: Appliances, Automotive, Document Processing Equipment, Industrial, Medical, Transportation.
Information provided by Saint Gobain Performance Products.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield <= 32130 psiASTM D-882
Flexural Yield Strength <= 49500 psi
Flexural Modulus <= 2.72e+6 psi
Compressive Strength <= 29000 psi
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 570 °FUL-746 B

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aquabond Technologies Aquabond™ ABS-65 Water Soluble Adhesive and Bonding Thermoplastic
Kuraray SEPTON® S4030 Thermoplastic Rubber
Kuraray SEPTON® S2104 Thermoplastic Rubber
Kuraray SEPTON® S2063 Thermoplastic Rubber
Kuraray SEPTON® S2007 Thermoplastic Rubber

PSTGQZ107 / 68618

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.