MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Formosa Plastics TAIRILAC® AE8200 ABS
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Product Description: Extrusion Grade. Characteristics: Extrusion molding, Super high impact, High rigid.
Availability: Asia Pacific; Europe; North America
Features: Ultra High Impact Resistance; High Rigidity
Agency Rating: EC 1907/2006 (REACH)
RoHS Compliance: RoHS Compliant
UL File Number: E162823
Processing Method: Extrusion

Information provided by Formosa Chemicals & Fiber Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM D792
Melt Flow 17 g/10 min
@Load 10.0 kg,
Temperature 220 °C
17 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 102102ASTM D785
Tensile Strength 43.0 MPa6240 psiASTM D638
Flexural Strength 75.2 MPa10900 psiASTM D790
Flexural Modulus 2.26 GPa328 ksiASTM D790
Izod Impact, Notched 3.58 J/cm
@Thickness 6.35 mm
6.70 ft-lb/in
@Thickness 0.250 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 96.1 °C
@Temperature 80.0 °C,
Time 28800 sec
205 °F
@Temperature 176 °F,
Time 8.00 hour
Annealed; ASTM D648
 87.8 °C
@Thickness 12.7 mm
190 °F
@Thickness 0.500 in
Unannealed; ASTM D648
Vicat Softening Point 100 °C
@Load 1.02 kg
212 °F
@Load 2.25 lb
ASTM D1525
Flammability, UL94  HB
@Thickness 1.52 mm
HB
@Thickness 0.0600 in
All Color
 HB
@Thickness 3.05 mm
HB
@Thickness 0.120 in
All Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFPCPD003 / 268117

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.