MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Stanyl® 46HF5041LW Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 46 (PA46); Nylon 46, Glass Fiber Reinforced

Material Notes: Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:
  • Highest mechanical properties at high temperatures
  • Excellent resistance to wear and low friction
  • Outstanding flow for easy processing and exceptional design freedom
  • Stanyl High Flowgrades that match the best flowing LCPs while maintaining a high level of mechanical properties

Key Applications:

  • Automotive: Powertrain components, Charge-air coolers, EPS and ETC gears, Motor Sensors, Auto connectors, Chain tensioners
  • E&E: Connectors, Microswitches, Bobbins, Memory modules, Motor components, Industrial, Specialty films and fibers, Consumer appliances

    Information provided by DSM.

    Former DSM Engineering Plastics product line is now with Envalior.

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 1.87 g/ccISO 1183
    Moisture Absorption at Equilibrium 1.1 %Humidity Absorption; Sim. to ISO 62
    Viscosity Number 70 cm³/g
    Linear Mold Shrinkage, Flow 0.0030 cm/cmISO 294-4
    Linear Mold Shrinkage, Transverse 0.0070 cm/cmISO 294-4
     
    Mechanical PropertiesOriginal ValueComments
    Tensile Strength at Break 150 MPaISO 527-1/-2
    Elongation at Break 1.3 %ISO 527-1/-2
    Tensile Modulus 16.0 GPaISO 527-1/-2
    Charpy Impact Unnotched 2.50 J/cm²
    @Temperature 23.0 °C
    ISO 179/1eU
    Charpy Impact, Notched 0.800 J/cm²
    @Temperature 23.0 °C
    ISO 179/1eA
     
    Electrical PropertiesOriginal ValueComments
    Comparative Tracking Index 250 - 399 VPLC 2; UL 746A
     
    Thermal PropertiesOriginal ValueComments
    CTE, linear, Parallel to Flow 20.0 µm/m-°C
    @Temperature 20.0 °C
    ISO 11359-1/-2
    CTE, linear, Transverse to Flow 80.0 µm/m-°C
    @Temperature 20.0 °C
    ISO 11359-1/-2
    Melting Point 295 °C10°C/min; ISO 11357-1/-3
    Deflection Temperature at 0.46 MPa (66 psi) 290 °CISO 75-1/-2
    Deflection Temperature at 1.8 MPa (264 psi) 270 °CISO 75-1/-2
    Vicat Softening Point 290 °C50°C/h 50N; ISO 306
    Glass Transition Temp, Tg 75.0 °CGlass Transition Temperature (10°C/min); ISO 11357-1/-2
    UL RTI, Electrical 140 °C
    @Thickness 1.50 mm
    UL746B
     140 °C
    @Thickness 0.750 mm
    UL746B
    UL RTI, Mechanical with Impact 110 °C
    @Thickness 0.750 mm
    UL746B
     125 °C
    @Thickness 1.50 mm
    UL746B
    UL RTI, Mechanical without Impact 120 °C
    @Thickness 0.750 mm
    UL746B
     125 °C
    @Thickness 1.50 mm
    UL746B
    Flammability, UL94 V-0
    @Thickness 0.400 mm
    IEC 60695-11-10
     V-0
    @Thickness 1.60 mm
    IEC 60695-11-10
    Glow Wire Ignition Temperature 825 °C
    @Thickness 0.750 mm
    IEC 60695-2-13
     925 °C
    @Thickness 3.00 mm
    IEC 60695-2-13
    Glow Wire Flammability Index 960 °C
    @Thickness 0.750 mm
    IEC 60695-2-12
     960 °C
    @Thickness 3.00 mm
    IEC 60695-2-12
     
    Descriptive Properties
    Flame RetardantYes
    Flame Retarding AgentYes
    Heat Stabilized or Stable to HeatYes
    Injection MoldingYes
    LubricantsYes
    PlatableYes
    Release AgentYes
    With FillersYes

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Envalior Stanyl® 46HF5040 (COND) Nylon 46 40% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow (North America)
    Envalior Stanyl® 46HF4130 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized, High Flow (North America)
    Envalior Stanyl® TE250F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized, Flame Retardant (North America)
    Envalior Stanyl® 46HF5041LW PA46-GF40 FR(17), Conditioned, 40% Glass Filled, Heat Stabilized, Flame Retardant
    Envalior Stanyl® 46HF5041LW Nylon 46-40% Glass Reinforced (European and Asian Grade) (Cond)

    PDSMEU450 / 31346

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.