MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik AquaSan Ni50 Covered electrodes
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: AquaSan Ni50 is a specially formulated, nickel based covered electrode with a waterproof coating for the welding of high strength steels with a Carbon Equivalent (CE) >0.4. AquaSan Ni50 is specified for welding base materials with a CE >0.4, which are susceptible to hydrogen embrittlement. Nickel has a high affinity for hydrogen and this composition allows hydrogen to diffuse into the weld metal and away from the high strength steel.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 648 MPa
Tensile Strength, Yield 524 MPa
@Strain 0.2 %
Elongation at Break 14 %
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.080 %
Chromium, Cr 12 %
Manganese, Mn 2.4 %
Nickel, Ni 64 %
Silicon, Si 0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical F3626E Solution Styrene Butadiene Rubber
Kuraray SEPTONĀ® 1050 Thermoplastic Rubber

NSANDV5046 / 199610

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.