Vydyne R515J NT0689 is a natural, 15% glass-filled, high-flow PA66 that is heat-stabilized with an electrically neutral heat stabilizer. It is specially designed for electrical applications requiring high dielectric strength, low conductivity and corrosion resistance.Information provided by Ascend Performance Materials. |