System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Guarniflon PTFE G458 Polytetrafluoroethylene 60% Bronze, 2% Carbon
Categories:
Polymer
;
Thermoplastic
;
Fluoropolymer
;
Polytetrafluoroethylene (PTFE)
;
Polytetrafluoroethylene (PTFE), Bronze Filled
Material Notes:
PTFE G Standard Compound with bronze
Properties: Enhanced compressive strength. Good wear resistance and high thermal conductivity.
Application: Unlubricated bearings for high speed excluding hard surfaces
Information provided by Guarniflon®
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
3.80
-
3.88
g/cc
extruded; ASTM D792
3.80
-
3.90
g/cc
molded; ASTM D792
Deformation
1.5 - 2.5 %
@Pressure 13.7 MPa,
Time 86400 sec
after 24hr relaxation; ASTM D621
5.0 - 6.0 %
@Pressure 13.7 MPa,
Time 86400 sec
ASTM D621
Mechanical Properties
Original Value
Comments
Hardness, Shore D
65 - 70
molded; ASTM D2240
65 - 70
extruded; ASTM D2240
Tensile Strength
>=
13.0
MPa
extruded; ASTM D4894, ASTM D4745
17.0
-
23.0
MPa
molded; ASTM D4894, ASTM D4745
Elongation at Break
>= 80 %
extruded; ASTM D4745
100 - 160 %
molded; ASTM D4894
Compressive Yield Strength
10.0
-
11.0
MPa
@Strain 1 %
ASTM D695
Coefficient of Friction, Dynamic
0.13
ASTM D1894
K (wear) Factor
>=
10.0
x 10
-8
mm³/N-M
at PV 100; ASTM D3702
Thermal Properties
Original Value
Comments
CTE, linear
80.0
-
90.0
µm/m-°C
ASTM D696
Maximum Service Temperature, Air
260
°C
Minimum Service Temperature, Air
-200
°C
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
AGC Fluon® PB3060 60% Bronze, PTFE Filled Compound
AGC FC 446 PTFE, 60% Bronze
Adamas Adalon® 805 PTFE, 40% Bronze
AGC FC 146 PTFE, 60% Bronze
AGC Fluon® FC 446 PTFE, 60% Bronze Powder Filled
PGUARN011 / 142744
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.