MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Iran Petrochemical (PCC) S 28 F Polypropylene Film
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Biaxially oriented poly propylene films suitable for metallization

Applications: cosmetics , food stuffs , lamination and other flexible films.

Information provided by Iran Petrochemical Commercial Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccISO 1183
Melt Flow 2.0 g/10 minISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 71ISO 868
Tensile Stress 35.0 MPaISO R527
Elongation at Yield 13 %ISO R527
Flexural Modulus 1450 MPaISO 178
Izod Impact, Notched (ISO) 6.50 kJ/m²ISO 180
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 155 °CISO 306/A
Heat Distortion Temperature 105 °CISO 75/B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) PC 1218 Polycarbonate
Iran Petrochemical (PCC) T 30 S Polypropylene
Iran Petrochemical (PCC) Moplen Z 30 S Polypropylene
Iran Petrochemical (PCC) S 30 S Polypropylene
Iran Petrochemical (PCC) S 30 G Polypropylene

PIPC301 / 149735

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.