MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
20/80 (80Pb-20Sn) Solder- ASTM B 32 Grade Sn20A and Grade 20B, UNS L54711
Categories: Metal; Nonferrous Metal; Lead Alloy; Solder/Braze Alloy

Key Words: Tin Alloys; Lead Alloys; Solder Alloy 20B; FED QQ-S-571 (Pb80)
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 10.2 g/cc
Viscosity 62900 cP
@Temperature 280 °C
Surface Tension 467 dynes/cm
@Temperature 280 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 11.3
Tensile Strength, Ultimate 40.0 MPa
Elongation at Break 16 %in 50 mm
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000198 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 26.5 µm/m-°C
@Temperature 15.0 - 110 °C
Thermal Conductivity 37.0 W/m-K
Melting Point 183 - 277 °C
Solidus 183 °C
Liquidus 277 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.005 %
Antimony, Sb 0.20 - 0.50 %
Arsenic, As <= 0.02 %
Bismuth, Bi <= 0.25 %
Copper, Cu <= 0.08 %
Iron, Fe <= 0.02 %
Lead, Pb 80 %
Tin, Sn 20 %target
Zinc, Zn <= 0.005 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
75Pb-25Sn Solder, ASTM Class 25A
10/90 (90Pb-10Sn) Solder - ASTM B32 Grade Sn10A, UNS L54520
68.4Pb-30Sn-1.6Sb Tin-Lead-Antimony Solder, ASTM Class 30C
20% Tin Solder (UNS L54710)
30/70 (70Pb-30Sn) Solder- ASTM B 32 Grade Sn30A, UNS L54820

MLSS20 / 12259

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.