MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Interam™ E-5A-4 Endothermic Mat
Categories: Other Engineering Material

Material Notes: When properly installed, 3M Interam Endothermic Mat E-5A-4 provides a uniform covering that, when exposed to high temperatures, releases chemically-bound water to cool the outer surfaces of the wrap material and significantly retard heat transfer. Helps protect structural steel components for up to four hours, critical electrical components for up to three hours and wall opening membranes for up to two hours. Applied to the back and sides of metallic utility boxes, this product helps achieve and equal F-rating and T-rating in membrane penetrations of rated wall assemblies. 3M Interam Endothermic Mat E-5A-4 is non-flame supporting with low-smoke evolution. The mat is flexible which aids in installation and allows it to more easily be applied on complex shapes and around corners.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.865 g/cc
Loss On Ignition 28 %
Thickness 408 mil
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 0.758 MPa
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.16 J/g-°C
@Pressure 91.2 MPa,
Temperature 24.0 °C
 1.39 J/g-°C
@Pressure 20.3 MPa,
Temperature 24.0 °C
Thermal Conductivity 0.100 W/m-K
@Temperature 316 °C
 0.118 W/m-K
@Temperature 399 °C
 0.140 W/m-K
@Temperature 482 °C
 0.151 W/m-K
@Temperature 93.0 °C
 0.179 W/m-K
@Temperature 177 °C
 
Descriptive Properties
AppearanceSilver exterior, white interior

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Thermatex 850 Paper Thermal Ceramic

PMM35448 / 170195

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.