MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
American Elements Beryllium Nanoparticles
Categories: Metal; Nonferrous Metal; Pure Element

Material Notes: General Description

Beryllium (Be) Nanoparticles, nanodots or nanopowder are spherical black high surface area particles. Nanoscale Beryllium Particles are typically 20-60 nanometers (nm) with specific surface area (SSA) in the 30 – 70 m 2 /g range. Nano Beryllium Particles are also available in Ultra high purity and high purity and coated and dispersed forms. Applications for Beryllium nanocrystals generally involve their use the study the toxicological effects of beryllium and in coatings, plastics, nanowire, nanofiber and textiles and in certain alloy and catalyst applications.

Key Words: Formula: Be; CAS Number: 7440-41-7
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size 0.020 - 0.060 µm
Specific Surface Area 30 - 70 m²/g
Molecular Weight 9.01 g/mol
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco Dura-Lith® NLGI 00 Grease EP
AISI 1060 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
Overview of materials for Epoxy, Cast, Unreinforced
Materion S-200-F C Beryllium

EJAMER10 / 5493

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.