MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Westlake Plastics

Westlake Plastics Absylux® SD-A Acrylonitrile-Butadiene-Styrene (anti-static)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Absylux® ABS SD-A is a permanently antistatic Acrylonitrile Butadiene Styrene with surface resistivity of 10E9 – 10E11 ohm/sq. The material is a non-carbon filled product, available in both natural and black color. It is ideal for protection against static discharge in electronic applications where contamination from potential sloughing of carbon powder would be of concern. Absylux® ABS SD-A is easy to machine and fabricate.

Industry: Engineering; Semiconductor and ESD

Colors Available: Black, Natural

Attributes: Dimensional Stability; Impact Resistance; Dielectric Properties

Shapes: Compression Sheet; Extruded Film; Extruded Rod

Information provided by Westlake Plastics Co.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 41.0 MPa5950 psiASTM D638
Elongation at Yield >= 10 %>= 10 %ASTM D638
Tensile Modulus 1.93 GPa280 ksiASTM D638
Flexural Yield Strength 69.0 MPa10000 psiASTM D790
Flexural Modulus 2.068 GPa299.9 ksiASTM D790
Izod Impact, Notched 1.33 J/cm2.49 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+9 - 1.00e+11 ohm1.00e+9 - 1.00e+11 ohmdry; ASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 76.0 °C169 °FASTM D648
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake Plastics Absylux® FR Acrylonitrile-Butadiene-Styrene Flame Retardant
A. Schulman Diamond ABSPC 7030 ABS/PC Injection Molding Grade, High Impact
Westlake Plastics Zelux® SD-P Polycarbonate (static dissipative)
Avient Edgetek® X AS/018 White Acrylonitrile Butadiene Styrene (ABS)
Multibase Multi-ABS 802 Utility Grade White

PWEST040 / 72720

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.