MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
Categories: Polymer; Thermoplastic; ASA Polymer; Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 - 1.24 g/ccAverage value: 1.07 g/cc Grade Count:176
Water Absorption 0.300 - 0.350 %Average value: 0.307 % Grade Count:15
Moisture Absorption at Equilibrium 0.300 - 0.350 %Average value: 0.344 % Grade Count:9
Water Absorption at Saturation 1.65 %Average value: 1.65 % Grade Count:8
Maximum Moisture Content 0.0100 - 0.0500Average value: 0.0290 Grade Count:21
Linear Mold Shrinkage 0.00100 - 0.0100 cm/cmAverage value: 0.00548 cm/cm Grade Count:139
 0.00500 - 0.00500 cm/cm
@Temperature 80.0 - 80.0 °C
Average value: 0.00500 cm/cm Grade Count:2
Linear Mold Shrinkage, Transverse 0.00200 - 0.00900 cm/cmAverage value: 0.00665 cm/cm Grade Count:13
 0.00500 - 0.00500 cm/cm
@Temperature 80.0 - 80.0 °C
Average value: 0.00500 cm/cm Grade Count:2
Melt Flow 0.200 - 45.0 g/10 minAverage value: 8.74 g/10 min Grade Count:174
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 75.0 - 119Average value: 101 Grade Count:105
Ball Indentation Hardness 65.0 - 100 MPaAverage value: 85.6 MPa Grade Count:9
Tensile Strength, Ultimate 29.4 - 75.5 MPaAverage value: 45.0 MPa Grade Count:49
Tensile Strength, Yield 15.0 - 83.4 MPaAverage value: 44.3 MPa Grade Count:148
Elongation at Break 3.00 - 230 %Average value: 33.3 % Grade Count:106
Elongation at Yield 2.50 - 45.0 %Average value: 4.95 % Grade Count:43
Modulus of Elasticity 1.45 - 2.80 GPaAverage value: 2.13 GPa Grade Count:65
Flexural Yield Strength 40.7 - 115 MPaAverage value: 68.9 MPa Grade Count:112
Flexural Modulus 0.220 - 5.98 GPaAverage value: 2.20 GPa Grade Count:149
Izod Impact, Notched 0.320 - 5.87 J/cmAverage value: 1.87 J/cm Grade Count:116
 0.270 - 0.570 J/cm
@Temperature -40.0 - -30.0 °C
Average value: 0.457 J/cm Grade Count:6
 0.196133 - 1.90249 J/cm
@Temperature -30.0 - -30.0 °C
Average value: 0.457 J/cm Grade Count:13
 0.196133 - 1.90249 J/cm
@Thickness 3.17 - 6.40 mm
Average value: 0.457 J/cm Grade Count:13
Izod Impact, Notched (ISO) 7.00 - 42.0 kJ/m²Average value: 15.4 kJ/m² Grade Count:29
 3.00 - 16.0 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 5.82 kJ/m² Grade Count:17
Izod Impact, Unnotched (ISO) 80.0 kJ/m² - NBAverage value: 85.0 kJ/m² Grade Count:5
 40.0 - 45.0 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 41.3 kJ/m² Grade Count:4
Charpy Impact Unnotched 3.50 J/cm² - NBAverage value: 7.81 J/cm² Grade Count:28
 1.50 J/cm² - NB
@Temperature -40.0 - -20.0 °C
Average value: 4.16 J/cm² Grade Count:12
Charpy Impact, Notched 0.700 - 5.77 J/cm²Average value: 1.79 J/cm² Grade Count:55
 0.110 - 1.60 J/cm²
@Temperature -40.0 - -20.0 °C
Average value: 0.494 J/cm² Grade Count:35
Instrumented Impact Total Energy 3.62 - 32.7 JAverage value: 20.9 J Grade Count:4
Instrumented Impact Energy at Peak 10.0 - 51.0 JAverage value: 36.0 J Grade Count:4
Tensile Creep Modulus, 1 hour 1850 - 2200 MPaAverage value: 2020 MPa Grade Count:3
Tensile Creep Modulus, 1000 hours 1100 - 1650 MPaAverage value: 1330 MPa Grade Count:6
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+12 - 1.00e+15 ohm-cmAverage value: 2.35e+14 ohm-cm Grade Count:27
Surface Resistance 1.10e+11 - 1.00e+15 ohmAverage value: 1.34e+14 ohm Grade Count:20
Dielectric Constant 3.40 - 3.90Average value: 3.73 Grade Count:7
Dielectric Strength 15.7 - 27.0 kV/mmAverage value: 21.4 kV/mm Grade Count:4
Dissipation Factor 0.00900 - 0.0340Average value: 0.0173 Grade Count:9
Arc Resistance 60.0 - 180 secAverage value: 105 sec Grade Count:4
Hot Wire Ignition, HWI 3.00 - 60.0 secAverage value: 18.6 sec Grade Count:6
High Amp Arc Ignition, HAI 0.000 - 120 arcsAverage value: 102 arcs Grade Count:6
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.2 - 121 µm/m-°CAverage value: 91.1 µm/m-°C Grade Count:45
CTE, linear, Transverse to Flow 86.4 - 116 µm/m-°CAverage value: 103 µm/m-°C Grade Count:6
Thermal Conductivity 0.170 W/m-KAverage value: 0.170 W/m-K Grade Count:9
Hot Ball Pressure Test 75.0 - 95.0 °CAverage value: 91.3 °C Grade Count:8
Deflection Temperature at 0.46 MPa (66 psi) 80.0 - 110 °CAverage value: 96.4 °C Grade Count:57
Deflection Temperature at 1.8 MPa (264 psi) 39.4 - 115 °CAverage value: 87.8 °C Grade Count:162
Vicat Softening Point 85.0 - 133 °CAverage value: 101 °C Grade Count:157
UL RTI, Electrical 50.0 °CAverage value: 50.0 °C Grade Count:6
UL RTI, Mechanical with Impact 50.0 °CAverage value: 50.0 °C Grade Count:6
UL RTI, Mechanical without Impact 50.0 °CAverage value: 50.0 °C Grade Count:5
Flammability, UL94 HB - 5VAGrade Count:85
Glow Wire Test 600 - 750 °CAverage value: 674 °C Grade Count:11
 
Optical PropertiesOriginal ValueComments
Haze 1.00 - 8.00 %Average value: 4.92 % Grade Count:5
Gloss 20.0 - 96.5 %Average value: 71.7 % Grade Count:9
Transmission, Visible 85.5 - 90.0 %Average value: 88.1 % Grade Count:5
 
Processing PropertiesOriginal ValueComments
Processing Temperature 200 - 280 °CAverage value: 236 °C Grade Count:6
Nozzle Temperature 190 - 271 °CAverage value: 238 °C Grade Count:37
Adapter Temperature 200 - 250 °CAverage value: 222 °C Grade Count:7
Die Temperature 200 - 250 °CAverage value: 229 °C Grade Count:7
Melt Temperature 170 - 280 °CAverage value: 232 °C Grade Count:86
Mold Temperature 37.8 - 90.0 °CAverage value: 61.1 °C Grade Count:85
Injection Velocity 200 mm/secAverage value: 200 mm/sec Grade Count:14
Roll Temperature 60.0 - 100 °CAverage value: 81.4 °C Grade Count:7
Drying Temperature 70.0 - 100 °CAverage value: 82.0 °C Grade Count:81
Moisture Content 0.0200 - 0.200 %Average value: 0.0932 % Grade Count:31
Injection Pressure 60.0 - 147 MPaAverage value: 72.1 MPa Grade Count:14

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for ASA/AES, Unreinforced, Extruded/Molded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
Overview of materials for Acetal Copolymer, Unreinforced
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced

O4960 / 78443

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.