MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Reynolds Free Form™ AIR FAST Epoxy putty
Categories: Polymer; Thermoset; Epoxy

Material Notes: Product Overview: Free Form™ AIR FAST is an easy to use epoxy putty that cures in minutes to a hard, strong and extremely lightweight plastic. Parts A and B are dispensed in equal amounts and mixed by hand. Used at room temperature, working time is 6 minutes in a 60 gram mass (2 oz) and handling time is 30 minutes (tack-free, hard surface). Epoxy putty is easy to color with UVO™ color pigments. You can smooth, texture, sculpt, or stamp while epoxy putty is in its “green” state. Cured epoxy is lightweight enough to float in water and can be easily carved, sanded, tooled and painted for finishing. It is compatible with original Free Form™ AIR, Free Form™ AIR HT and Free Form™ AIR Fire Safe.

Applications: Free Form™ AIR FAST is used for fast “rough shaping” projects, filling in voids and repair applications. Epoxy will bond to a variety of plastics (urethane, PVC, etc.) metals, wood, EPS foam, paper, ceramics, plaster, etc. It can be used for a variety of fast repair applications including marine repairs; it will cure under water. Epoxy Tooling - use as a filleting material or for jig/fixture construction. Laminating - Free Form™ AIR FAST putty in between layers of EpoxAmite™ Laminating Epoxy and fiberglass cloth, carbon or other fiber for making lightweight composite parts.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.450 g/ccASTM D-1475
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60ASTM D2240
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 63.0 °CHeat Deflection Temperature; ASTM D-648
 
Descriptive Properties
Buoyant Force:166.5 kg /m3
ColorGrey
Mix Ratio1A:1Bby volume
Mixed ViscosityDough
Specific Volume61.6[in3/lb], ASTM D1475

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREYN295 / 296996

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.