MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Bormed™ RG835MO Polypropylene Copolymer for Healthcare Applications
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Bormed RG835MO is specially modified polypropylene random copolymer with high melt flow intended for use in medical and medical related articles. RG835MO is modified with an internal lubricant for products requiring a low surface friction.

Bormed RF830MO is designed for use in devices such as syringes and needle hubs, blood and urine tubes, catheter connections, and screw caps and closures.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccISO 1183
Melt Flow 30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 90ISO 2039-2
Tensile Strength, Yield 3988 psiAt 50 mm/min; ISO 527-2
Elongation at Yield 12 %At 50 mm/min; ISO 527-2
Tensile Modulus 1.20 GPaAt 1 mm/min; ISO 527-2
Charpy Impact, Notched 0.600 J/cm²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °CISO 75-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 - 250 °C
Mold Temperature 30.0 - 40.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Bormed™ RF830MO Polypropylene Copolymer for Healthcare Applications
Borealis Bormed™ RF825MO Polypropylene Copolymer for Healthcare Applications
Borealis Bormed™ HF840MO Polypropylene Homopolymer for Medical Applications
Borealis Bormed™ HF855MO Polypropylene Homopolymer for Medical Applications
Borealis Bormed™ HD810MO Polypropylene Copolymer for Medical Applications

PBOREA083 / 27390

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.