MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 35% Cold Worked
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Data provided by Carpenter Technology Corporation.

Medical Implant Alloy. Vacuum arc remelted (VAR), low carbon version of Type 316 stainless. The secondary premium melting step (VAR) imparts improved cleanliness. The chemistry modifications are designed to maximize the corrosion resistance of this alloy and provide a ferrite free microstructure. The alloy is nonmagnetic even after severe cold forming operations.

BioDur™ is a trademark of Carpenter Technology Corporation.

Key Words: ASTM F138 Grade 2; ASTM F139 Grade 2; ISO 5832-1 Composition D; Type 316 Stainless Steel
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.95 g/cc0.287 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 266266Estimated from Rockwell C for Brinell test with 3000 kg load, 10 mm ball.
Hardness, Knoop 289289Estimated from Rockwell C
Hardness, Rockwell C 2626
Hardness, Vickers 280280Estimated from Rockwell C
Tensile Strength, Ultimate 862 MPa125000 psi
Tensile Strength, Yield 793 MPa
@Strain 0.2 %
115000 psi
@Strain 0.2 %
Elongation at Break 18 %18 %
Reduction of Area 72 %72 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000740 ohm-cm0.0000740 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.5 µm/m-°C
@Temperature 0.000 - 649 °C
10.3 µin/in-°F
@Temperature 32.0 - 1200 °F
Specific Heat Capacity 0.500 J/g-°C0.120 BTU/lb-°F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.030 %<= 0.030 %
Chromium, Cr 17 - 19 %17 - 19 %
Copper, Cu <= 0.50 %<= 0.50 %
Iron, Fe 62 %62 %as remainder
Manganese, Mn <= 2.0 %<= 2.0 %
Molybdenum, Mo 2.25 - 3.5 %2.25 - 3.5 %
Nickel, Ni 13 - 15 %13 - 15 %
Nitrogen, N <= 0.10 %<= 0.10 %
Phosphorus, P <= 0.025 %<= 0.025 %
Silicon, Si <= 0.75 %<= 0.75 %
Sulfur, S <= 0.010 %<= 0.010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, Annealed
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 90% Cold Worked
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 48% Cold Worked
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 52% Cold Worked
Kinetics MIM 316 Stainless Steel (Standard Grade)

NCAR51 / 15629

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.