MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Braskem HS5608 Blown Molding High Density Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Description: HS5608 is a high-density polyethylene with high molecular weight, copolymer. Offers good processability, outstanding stress cracking resistance (ESCR), excellent stiffness and impact strength. Suitable for blow molding of large volumes

Application: Typical blow molded applications include containers and drums from 20 to 200 liters, for chemical, agrochemical and food package.

Information provided by Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.955 g/ccASTM D792
ESCR 100% Igepal® >= 1000 hour
@Temperature 50.0 °C
F50, molded 2 mm, 0.3 mm notched-plaques; ASTM D1693
ESCR 10% Igepal® 200 hour
@Temperature 50.0 °C
F50, molded 2 mm, 0.3 mm notched-plaques; ASTM D1693
Melt Flow 0.30 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ASTM D1238
 8.5 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 35.0 MPaASTM D638
Flexural Modulus, 1% Secant 1350 MPaASTM D790
Impact 200
@Temperature -40.0 °C
[J/m], Charpy; ASTM D6110
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 73.0 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Feed Temperature 180 - 190 °C
Die Temperature 210 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total MDPE 3802 Medium Density Polyethylene, Cable
INEOS Styrolution PS 6220 HIPS
Chevron Phillips Marlex® C590 High Density Polyethylene
Braskem HS5407 Blown Molding High Density Polyethylene
Braskem GV0350 HDPE Blow Molding Polyethylene Copolymer

PBRASK2091 / 199972

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.