MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Geniosil® GF 9 Silane
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoset; Polysulfide Sealant/Adhesive

Material Notes: Empirical formula: C8H22N2O3Si

CAS No.: 1760-24-3

Properties: Thanks to the specific reactivity of the 2- aminoethylaminopropyl structure, using GENIOSIL® GF 9 as an adhesion promoter in glass-fiber reinforced or filler-modified plastics reduces the filler's sedimentation tendency and improves dispersibility and numerous mechanical properties (e.g. flexural strength, tensile strength, modulus of elasticity) of the composites. The use of GENIOSIL® GF 9 in these materials also results in a markedly improved resistance to water (vapor) and corrosion. Electrical properties, such as volume resistivity and the dielectric constant, are also positively influenced

Special features: Due to the nature of the amino group, this substance reacts as a strong base. The silane hydrolyzes autocatalytically in the presence of moisture (methanol is released) to form silanols, which can subsequently react with themselves to produce siloxanes or can bind to inorganic substrates. It´s a clear, colorless to light yellow liquid with a characteristic amine odor. As a typical amine, GENIOSIL® GF 9 can also interact with numerous organic polymers and thus function as a molecular bridge between organic and inorganic substrates.

Application: GENIOSIL® GF 9 is mainly used as a surface modifier for glass fibers, glass-fiber fabrics, fillers (e.g. glass or mineral wool, mica, talc, wollastonite, kaolin, christobalite, metal oxides) and pigments used in various plastics, including epoxy resins, polyamides, polyacrylates, polyurethanes, ethylene/vinyl acetate copolymers and many others. Other important applications include its uses as an adhesion promoter in polysulfides and phenolic resins for abrasives and insulating materials and as a primer for sealants, adhesives and coatings.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/cc
@Pressure 0.1013 MPa
DIN 51757
Molecular Weight 222.4 g/mol
 
Thermal PropertiesOriginal ValueComments
Boiling Point >= 147 °C
@Pressure 0.00160 MPa
DU-GL A2
Flash Point >= 100 °CEN 22719
Ignition Temperature 300 °Cliquids; DIN 51794
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.445
 
Descriptive Properties
Active ingredients>98
Content8.3 meq/gAmine

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dymax 3073 Solvent-Free Plastic Adhesive
Dow Bynel® 30E753 Anhydride Modified Ethylene Vinyl Acetate
Morgan Advanced Ceramics Firemaster Board 350 Thermal Ceramic
LyondellBasell Plexar® PX5125 Extrudable Tie-Layer Resin - Anhydride Modified LLDPE
Morgan Advanced Ceramics Green Glass Paper Thermal Ceramic

PWACK9308 / 204837

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.