MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Henkel Loctite® Nuva-Sil® 5091 High Adhesion Potting
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes:
Potters and Silicon Light Cure Adhesives
Loctite® Potting materials are used on electronic device housings to enhance mechanical strength, provide electrical insulation and enhance vibration and shock resistance of assemblies.

For electronics assembly, Loctite offers deep potting, high adhesion, non-corrosive, and thermally conductive potting products. These can be cured with heat, UV light, or moisture.

Loctite® 5091 Nuva-Sil® High Adhesion Potting
A UV curing silicon for high speed shallow potting, coating and sealing of electronic connectors. High adhesion for difficult-to-bond substrates. Key Substrates: Glass, Metal, Ceramic Cure Type: Ultraviolet, Moisture, Methoxy Bonding Type: Silicone

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 5500 cP
@Temperature 25.0 °C
5500 cP
@Temperature 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3434
Elongation at Break 100 %100 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C350 °F
Minimum Service Temperature, Air -53.9 °C-65.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1.00 min0.0167 hourat 40 mW/cm^2
 
Descriptive Properties
ColorTranslucent/Colorless

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NeXolve LaRC™-CP1 Polyimide
Henkel Loctite® 5083 Silicone Light Cure Adhesive
Momentive Performance Materials RTV123 Black Adhesive Sealant, General Purpose Paste
Momentive Performance Materials RTV103 One Component Acetoxy Adhesive Sealant, Black
Chemical Concepts PERMATEX® #26 High-Temp RTV Silicone Gasket

PLOCT202 / 51938

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.