MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC ULTEM™ Resin JD7904 Polyetherimide (PEI)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: ULTEM JD7904 compound is based on Polyetherimide (PEI) resin containing conductive carbon powder. Added features of this grade include: Anti-Static, Anti-Dust.

Features: Electrically Conductive,Antistatic

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.31 g/cc1.31 g/ccASTM D792
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 84.0 MPa12200 psiSABIC - Japan Method
Elongation at Break 4.0 %4.0 %SABIC - Japan Method
Flexural Strength 127 MPa18400 psiASTM D790
Flexural Modulus 3.72 GPa540 ksiASTM D790
Izod Impact Notched 29.0 J21.4 ft-lbASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+10 ohm1.00e+10 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 200 °C
@Thickness 3.20 mm
392 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 380 - 405 °C716 - 761 °F
Zone 2 370 - 400 °C698 - 752 °F
Zone 3 380 - 410 °C716 - 770 °F
Melt Temperature 380 - 410 °C716 - 770 °FInjection Molding
Mold Temperature 140 - 170 °C284 - 338 °F
Drying Temperature 150 °C302 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
Back Pressure 5.00 - 10.0 MPa725 - 1450 psi
Shot Size 40 - 70 %40 - 70 %
 
Descriptive Properties
Screw speed (Circumferential speed)0.1-0.2 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82733 / 290680

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.