MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Ovation Polymers Nemcon™ H ABS DP116P ABS
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: ABS-Thermally conducting, electrically insulating grade with high HDT and improved processability.

Information provided by Ovation Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.66 g/ccASTM D792
Maximum Moisture Content 0.020%
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 32.0 MPa50 mm/min; ASTM D638
Elongation at Break 1.7 %50 mm/min; ASTM D638
Tensile Modulus 3.572 GPa50 mm/min; ASTM D638
Flexural Strength 52.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3.188 GPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 21.4 J/m
@Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 8.00e+12 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.700 W/m-KASTM E-1461
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 220 - 270 °C
Zone 1 220 - 255 °C
Zone 2 220 - 260 °C
Zone 3 220 - 265 °C
Melt Temperature 220 - 275 °C
Mold Temperature 40.0 - 80.0 °C
Drying Temperature 70.0 - 90.0 °C
Dry Time 4 - 6 hour
Back Pressure 30.0 - 80.0 psi
Screw Speed 70 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ovation Polymers Nemcon™ E ABS 20CF
Ovation Polymers SOFTAPLAS™ S 75A Thermoplastic Elastomer
Ovation Polymers Nemcon™ E HDPE 11000
Ovation Polymers Nemcon™ E PC 08CF Polycarbonate
Ovation Polymers Nemcon™ E PET 30131 PET

POVAT124 / 55837

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.