MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PPR 7425 Polypropylene, Injection Molding Grade
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Random copolymer for injection molding

Clarity - FINA 7425, a random copolymer, exhibits excellent clarity when molded in polished molds.

Impact - FINA 7425 produced molded parts with measurably improved impact compared with parts molded from polypropylene homopolymers.

FDA - FINA 7425 complies with all applicable FDA regulations for food contact applications.

Recommended Applications - FINA 7425 is recommended for injection molding medical devices and disposables, clear food containers and specialty housewares.

Processing - FINA 7425 resin processes on conventional injection molding equipment with typical melt temperatures of 390-450°F (200-232°C)

Data provided by the manufacturer, Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 4.0 g/10 minASTM D1238L
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 85ASTM D288A
Tensile Strength, Ultimate 22.1 MPaASTM D638
Elongation at Break 11 %ASTM D638
Modulus of Elasticity 0.760 GPaASTM D638
Flexural Modulus 0.620 GPaASTM D790
Izod Impact, Notched 0.694 J/cmASTM D256A
Izod Impact, Unnotched NBASTM D256A
Impact Test 23.7 J
@Thickness 3.17 mm
Drop Impact, plaques. Fina API test
 
Thermal PropertiesOriginal ValueComments
Melting Point 145 °CDSC
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 232 °CInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPH 3620WZ Polypropylene, Injection Molding Grade
Total PPH 3720WZ Polypropylene, Injection Molding Grade
Total PPH 3429 Polypropylene, Injection Molding Grade
Total PPH 3622 Polypropylene, Injection Molding Grade
Total PPH 3825 Polypropylene, Injection Molding Grade

PFIN45 / 38375

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.