Co-polymer nylon, GF reinforced, good appearance, high flow, GF 50%, PA-GF50. General Amilan™ Notes: AMILAN™ nylon (polyamide) is a thermoplastic engineering plastic containing an amide group (-CONH-) and it exhibits excellent strength, toughness, heat resistance, and anti-friction wear resistance. A variety of grades designed for various customer needs and applications are available. Information provided by Toray Resin Co. |