MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chi Mei Acryrex® CM-207 PMMA
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, General Purpose, Molded

Material Notes:
    Features:
  • General Purpose
  • Good Weather Resistance
  • High Gloss
  • High Heat Resistance
  • High Strength
  • Medium Viscosity
    Uses:
  • Automotive Interior Parts
  • Bathroom Accessories
  • Containers
  • Cosmetics
  • Household Goods
  • Knobs
RoHS Compliant

Appearance: Clear/Transparent

Forms: Pellets

Processing Method: Extrusion and Injection Molding

    Africa & Middle East
  • Asia Pacific
  • Europe
  • Latin America
  • North America
  • South America

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.700 g/cc0.0253 lb/in³Apparent; ASTM D1182
 1.19 g/cc0.0430 lb/in³ASTM D792
Water Absorption 0.30 %0.30 %Equilibrium; ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0060 cm/cm0.0020 - 0.0060 in/inASTM D955
Melt Flow 8.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
8.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 85
@Thickness 6.35 mm
85
@Thickness 0.250 in
ASTM D785
Tensile Strength, Yield 66.9 MPa
@Thickness 3.18 mm
9700 psi
@Thickness 0.125 in
6 mm/min; ASTM D638
Elongation at Break 5.0 %
@Thickness 3.18 mm
5.0 %
@Thickness 0.125 in
6 mm/min; ASTM D638
Flexural Strength 97.9 MPa
@Thickness 6.35 mm
14200 psi
@Thickness 0.250 in
2.8 mm/min; ASTM D790
Izod Impact, Notched 0.200 J/cm
@Thickness 6.35 mm
0.375 ft-lb/in
@Thickness 0.250 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.73.7ASTM D150
Dielectric Strength 31.0 kV/mm788 kV/inASTM D149
Dissipation Factor 0.190.19ASTM D150
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C
@Thickness 6.35 mm
198 °F
@Thickness 0.250 in
unannealed; ASTM D648
Vicat Softening Point 105 °C221 °F50°C/hr; ASTM D1525
Flammability, UL94 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
UL 94
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.491.49ASTM D542
Transmission, Visible 92 %
@Thickness 3.18 mm
92 %
@Thickness 0.125 in
ASTM D1003
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 185 - 200 °C365 - 392 °F
Middle Barrel Temperature 210 - 225 °C410 - 437 °F
Front Barrel Temperature 200 - 220 °C392 - 428 °F
Mold Temperature 40.0 - 60.0 °C104 - 140 °F
Drying Temperature 75.0 - 80.0 °C
@Time 14400 sec
167 - 176 °F
@Time 4.00 hour
 
Descriptive Properties
Power Factor0.5ASTM D150

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chi Mei Acryrex® CM-205 PMMA
Chi Mei Acryrex® CM-211 PMMA
Plaskolite West Optix® CA-1000 I Clear High Impact Acrylic Resin
Plaskolite West Optix® CP - 75 General Purpose Acrylic Resin
Chi Mei Wonderlite® PC-115 Polycarbonate

PCHI944 / 109432

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.