MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® 8254 HS BK-102 PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Ultramid 8254 HS is a highly flexible, heat stabilized, impact modified nylon 6 extrusion grade for tubing applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccISO 1183
Water Absorption 1.2 %24 hour; ISO Test
 7.1 %ISO 62
Moisture Absorption at Equilibrium 2.0 %23°C/50% R.H.; ISO 62
Linear Mold Shrinkage 0.013 cm/cmASTM Data; MD
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 40ASTM Test
Tensile Strength, Yield 34.0 MPa50mm/min; ISO 527
 34.0 MPa2 in/min; ASTM Test
 12.0 MPa
@Temperature 120 °C
ISO Data
 12.0 MPa
@Temperature 120 °C
ASTM Test
 15.0 MPa
@Temperature 80.0 °C
ASTM Test
 15.0 MPa
@Temperature 80.0 °C
ISO Data
 83.0 MPa
@Temperature -40.0 °C
ASTM Test
 83.0 MPa
@Temperature -40.0 °C
ISO Data
Elongation at Break >= 50 %50mm/min, Nominal strain; ISO 527
 >= 100 %2 in/min; ASTM Test
Elongation at Yield 7.0 %50mm/min; ISO 527
 30 %2 in/min; ASTM Test
 4.0 %
@Temperature -40.0 °C
ISO Data
 20 %
@Temperature 120 °C
ISO Data
Tensile Modulus 875 MPa1mm/min; ISO 527
 155 MPa
@Temperature 120 °C
ISO Data
 180 MPa
@Temperature 80.0 °C
ISO Data
 2730 MPa
@Temperature -40.0 °C
ISO Data
Flexural Strength 28.0 MPaASTM Test
Flexural Modulus 610 MPaASTM Test
 750 MPaISO Data
Izod Impact, Notched 6.40 J/cm
@Thickness 3.17 mm
ASTM Test
Izod Impact, Notched (ISO) NBISO Test
 6.00 kJ/m²
@Temperature -40.0 °C
ISO Test
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear 117 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM Test
CTE, linear, Parallel to Flow 93.0 µm/m-°CISO 11359
CTE, linear, Transverse to Flow 111 µm/m-°CISO 11359
Melting Point 220 °C10 K/min
 220 °CASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 119 °CISO 75
 124 °CASTM Test
Deflection Temperature at 1.8 MPa (264 psi) 43.0 °CISO 75
 47.0 °CASTM Test
Flammability, UL94 HB
 HB
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 °CInjection molding
Mold Temperature 70.0 °CInjection molding
 
Descriptive Properties
ColorBK-102
Commercial StatusActive America
FormPellets
Impact ModifiedYes
Primary Processing TechniqueExtrusion
ProcessingInjection Molding
 Other Extrusion
 Profile Extrusion
Special characteristicHeat stabilized or stable to heat
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® 8253 HS PA6 (Dry)
BASF Ultramid® 8350 HS PA6 (Dry)
Nylene® NX4301 Nylon 6, Extrusion Grade
BASF Ultramid® 8270 HS BK 102 PA6 (Dry)
BASF Ultramid® 8254 HS BK-102 PA6 (Conditioned)

PBASF9177 / 84941

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.