MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
ATI Allegheny Ludlum AL Altemp® 625 Nickel-Base Superalloy, UNS N06625
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Allegheny Ludlum Altemp 625 alloy is an austenitic nickel-base superalloy possessing excellent resistance to oxidation and corrosion over a broad range of corrosive conditions, including jet engine environments and in many other aerospace and chemical process applications. Specific uses include jet engine nacelles, engine plumbing, aircraft ducting, recuperators, and thrust reversers. The alloy has outstanding strength and toughness at temperatures ranging form cryogenic temperature to 1093°C. This alloy also has exceptional fatigue resistance.

The Altemp 625 alloy derives its strength from the solid solution strengthening effects of molybdenum and columbium on the nickel-chromium matrix. These elements also contribute to the alloy's outstanding corrosion resistance. Although the alloy was developed for high temperature strength, its highly alloyed composition provides a high level of general corrosion resistance to a wide range of oxidizing and non-molybdenum provide excellent resistance to chloride ion pitting and the high level of nickel provides resistance to chloride stress corrosion cracking.

The material posses a high degree of formability and shows better weldability than many high alloyed nickel-base alloys. The alloy is resistant to intergranular corrosion even in the welded condition.

Information provided by Allegheny Ludlum.

Key Words: DIN 2.4856; ASTM B-443; ASME SB-443; AMS 5599
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.44 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 95Typical Annealed
Tensile Strength, Ultimate >= 827 MPaFor flat products (<4" thickness) and seamless tube and pipe
Tensile Strength, Yield >= 414 MPaFor flat products (<4" thickness) and seamless tube and pipe
Elongation at Break 45 %Typical Annealed
 
Electrical PropertiesOriginal ValueComments
Magnetic Permeability 1.000675F; 200 Oe
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.410 J/g-°C
Melting Point 1280 - 1350 °C
Solidus 1280 °C
Liquidus 1350 °C
Maximum Service Temperature, Air 1093 °CExcellent oxidation and scale resistance to this temp.
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.30 %
Carbon, C 0.050 %
Chromium, Cr 22 %
Iron, Fe 4.0 %
Manganese, Mn 0.30 %
Molybdenum, Mo 9.0 %
Nickel, Ni 60 %as balance; includes Co
Niobium, Nb (Columbium, Cb) 3.5 %
Phosphorus, P 0.010 %
Silicon, Si 0.25 %
Sulfur, S 0.0030 %
Titanium, Ti 0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals INCONEL® Alloy 625
ATI Allvac® Nickelvac® 625 Nickel Superalloy, Heat Treatment: 927°C (1700°F) Anneal
Carlson C 625 Nickel-Chromium-Molybdenum Alloy
MetalTek MTEK 625 Cast UNS N26625 Severe Corrosion and Heat Resistant Alloy
Haynes 625 alloy, 0% cold reduction

NLN625 / 18020

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.