MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AGC Fluon® FC 111 PTFE, 5% Molybdenum Disulfide Filled
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Description: Fluon® FC 111 (310 111 020) is a 5% molybdenum disulfide filled PTFE product. This compound is supplied dry powder form.

End Uses: Molybdenum disulfide is added to PTFE to improve the wear properties, increase surface hardness, and decrease the coefficient of friction without sacrificing the chemical and thermal resistance of the polymer.

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.21 g/ccASTM D4745
Filler Content 5.0 %ASTM D4745
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 59Sustained; ASTM D2240
 61Peak; ASTM D2240
Tensile Strength 3900 psiASTM D4745
Elongation at Break 250 %ASTM D4745

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AGC FC 111 PTFE, 5% Moly
AGC FC 411 PTFE, 5% Moly
AGC Fluon® FC 174 PTFE, 15% Glass Fiber/ 5% Molybdenum Disulfide Filled
Cast Nylons Nycast® Nyloil®-MDX Lubricated Nylon, MoS2 Filled
Eifeler Coatings Technology MoST™ Molybdenum disulfide PVD Coating

PAGCX085 / 191194

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.