MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYLSTAR® AF 219 V30 PA 66 30% Glass Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled; Nylon 66, Heat Stabilized

Material Notes: Description: TECHNYLSTAR® AF 219 V30 is a polyamide 6.6, high flow, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black and natural color.

Key Properties: Easy processing; Heat stabilized; Suitable for Mucell®; Good surface aspect; Reduced electrolytic corrosion

Benefits: This product has enhanced molding behaviors and better surface aspect. It offers an excellent combination between thermal and mechanical properties. This grade restricts electrolytic corrosion.

Applications: This product can be used as insulation material for electronic application such as connectors or thin parts under stress.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.37 g/ccISO 1183/A
Water Absorption 0.80 %
@Time 86400 sec
ISO 62
Linear Mold Shrinkage 0.0062 cm/cmIsotropy
Linear Mold Shrinkage, Flow 0.0050 cm/cm
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 190 MPaISO 527 Type 1A
Elongation at Yield 3.0 %ISO 527 Type 1A
Tensile Modulus 10000 MPaISO 527 Type 1A
Flexural Strength 270 MPaISO 178
Flexural Modulus 9000 MPaISO 178
Charpy Impact Unnotched 70.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 600 VSol A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
ISO 11359
Melting Point 263 °CISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 258 °CISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 250 °CISO 75/Af
 
Processing PropertiesOriginal ValueComments
Processing Temperature 270 - 280 °CCompression zone
 280 - 290 °CMixing zone
Feed Temperature 260 - 270 °C
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Durethan® BKV 30 H2.0 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
Overview of materials for Nylon 66, 30% Glass Fiber Filled
Domo TECHNYLSTAR® AF 218 V30 BLACK 21N PA 66 30% Glass Reinforced, Conditioned
Domo TECHNYLSTAR® AF 218 V25 BLACK 21N PA 66 25% Glass Reinforced, Dry

PSOLVAY875 / 218603

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.