MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Vinnex® 2523 Vinyl Acetate Homopolymer
Categories: Polymer; Thermoplastic

Material Notes: VINNEX® 2523 is a solid, thermoplastic homopolymer. The clear and colorless resin is prepared by polymerization of vinyl acetate. VINNEX® 2523 is tasteless.

Application: Typical applications for VINNEX® 2523: blending with natural fibers or flour such as wood, starch and cork. It is also suitable for the modification of biopolymers and biopolymer compounds.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.700 - 0.850 g/ccDIN 53466
Density 1.18 g/ccDIN EN ISO 2811/1-3
Volatiles <= 1.0 %
Viscosity 8.0 - 11 cP10% in ethylacetate; ASTM D445-06
 640 cP
@Temperature 180 °C
 1500 cP
@Temperature 160 °C
 4000 cP
@Temperature 140 °C
Molecular Weight 130000 g/mol
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 0.50[mg KOH/g]
 
Thermal PropertiesOriginal ValueComments
Softening Point 120 °CRing and Ball; DIN ISO 4625
Glass Transition Temp, Tg 43.0 °CDIN EN ISO 11357-2
 
Descriptive Properties
K-Value48-54DIN 53726

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Vinnex® 2525 Vinyl Acetate Homopolymer
NatureWorks® Ingeo™ AW 240D Biopolymer for Food Serviceware
NatureWorks® Ingeo™ 6252D Meltblown Fiber Grade Biopolymer
NatureWorks® Ingeo™ 4043D General Purpose Film Grade Biopolymer
NatureWorks® Ingeo™ 4032D Film Grade PLA

PWACK9666 / 205195

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.