MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro MONDUR® TD-65 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Mondur TD-65 is a high, 2,6-isomer toluene diisocyanate.

Properties / Applications: Mondur TD-65 diisocyanate is used in the formulation of flexible polyester and polyether urethane foams and in the manufacture of prepolymer resins. As with any product, use of Mondur TD-65 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/cc
 
Thermal PropertiesOriginal ValueComments
Flash Point 127 °CPMCC
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.566
 
Descriptive Properties
Acidity<0.005%
AppearanceWater white to pale yellow liquid
Boling Point251°C
Color<20APHA
Content<0.01%Hydrolyzable chlorides
 >99.7%Assay
 33-35%2,6-Isomer ratio
 65-67%2,4-Isomer ratio
Crystallization21°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Hytrel® 7246 TPC-ET
Polyram PlusTek PB150 Nylon 6, Injection Molding
Huntsman IROGRAN® A 92 K 5031 TPU-High Temperature Performance
Huntsman IROGRAN® A 92 K 4107 TPU-High Temperature Performance
Ashley Polymers Ashlene® LT940H Nylon 11

PCOVEST0922 / 202705

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.