MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Aluminum 5050-H34
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 5000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A95050; ISO AlMg1.5; Aluminium 5050-H34; AA5050-H34; Al5050-H34
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.69 g/ccAA; Typical
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 53AA; Typical; 500 g load; 10 mm ball
Hardness, Knoop 68Converted from Brinell Hardness Value
Tensile Strength, Ultimate 28.0 ksiAA; Typical
 27.0 MPa
@Temperature 371 °C
 41.0 MPa
@Temperature 316 °C
 60.0 MPa
@Temperature 260 °C
 95.0 MPa
@Temperature 204 °C
 170 MPa
@Temperature 149 °C
 195 MPa
@Temperature -28.0 °C
 195 MPa
@Temperature 24.0 °C
 195 MPa
@Temperature 100 °C
 205 MPa
@Temperature -80.0 °C
 305 MPa
@Temperature -196 °C
Tensile Strength, Yield 24.0 ksiAA; Typical
 18.0 MPa
@Strain 0.2 %,
Temperature 371 °C
 29.0 MPa
@Strain 0.2 %,
Temperature 316 °C
 41.0 MPa
@Strain 0.2 %,
Temperature 260 °C
 50.0 MPa
@Strain 0.2 %,
Temperature 204 °C
 150 MPa
@Strain 0.2 %,
Temperature 149 °C
 165 MPa
@Strain 0.2 %,
Temperature -28.0 °C
 165 MPa
@Strain 0.2 %,
Temperature 24.0 °C
 165 MPa
@Strain 0.2 %,
Temperature 100 °C
 170 MPa
@Strain 0.2 %,
Temperature -80.0 °C
 205 MPa
@Strain 0.2 %,
Temperature -196 °C
Elongation at Break 8.0 %
@Thickness 1.59 mm
AA; Typical
Modulus of Elasticity 10000 ksiAA; Typical; Average of tension and compression. Compression modulus is about 2% greater than tensile modulus.
Ultimate Bearing Strength 345 MPaEdge distance/pin diameter = 2.0
Bearing Yield Strength 234 MPaEdge distance/pin diameter = 2.0
Poissons Ratio 0.33
Fatigue Strength 13000 psi
@# of Cycles 5.00e+8
completely reversed stress; RR Moore machine/specimen
Machinability 30 %0-100 Scale of Aluminum Alloys
Shear Modulus 25.9 GPa
Shear Strength 18.0 ksiAA; Typical
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 21.0 ohm-cir-mil/ft
@Temperature 20.0 °C
AA; Typical
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.2 µin/in-°F
@Temperature 20.0 - 100 °C
AA; Typical; average over range
 21.8 µm/m-°C
@Temperature -50.0 - 20.0 °C
 24.7 µm/m-°C
@Temperature 20.0 - 200 °C
 25.6 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.900 J/g-°C
Thermal Conductivity 1340 BTU-in/hr-ft²-°FAA; Typical at 77°F
Melting Point 1155 - 1205 °FAA; Typical range based on typical composition for wrought products >= 1/4 in. thickness
Solidus 1155 °FAA; Typical
Liquidus 1205 °FAA; Typical
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 650 °Fholding at temperature not required
Hot-Working Temperature 500 - 950 °F
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 96.3 - 98.9 %As remainder
Chromium, Cr <= 0.10 %
Copper, Cu <= 0.20 %
Iron, Fe <= 0.70 %
Magnesium, Mg 1.1 - 1.8 %
Manganese, Mn <= 0.10 %
Other, each <= 0.05 %
Other, total <= 0.15 %
Silicon, Si <= 0.40 %
Zinc, Zn <= 0.25 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 5050-H32
Aluminum 5050-H36
Aluminum 5050-H38
Aluminum 6061-T6; 6061-T651
Aluminum 5050-O

MA5050H34 / 9146

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.