MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Desmopan® 481 Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Injection molding grade; free from plasticizers; grease and oil-resistant; low compression set; high elasticity; good heat resistance; easy release; Application; roller coating; Seals, membranes; Automotive engineering

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8181ISO 868
Hardness, Shore D 3030ISO 868
Tensile Strength, Ultimate 36.8 MPa5340 psi200 mm/min; DIN 53504
Tensile Stress at Strain  1.30 MPa
@Strain 10 %
189 psi
@Strain 10 %
200 mm/min; DIN 53504
 3.80 MPa
@Strain 50 %
551 psi
@Strain 50 %
200 mm/min; DIN 53504
 5.20 MPa
@Strain 100 %
754 psi
@Strain 100 %
200 mm/min; DIN 53504
 9.00 MPa
@Strain 300 %
1310 psi
@Strain 300 %
ISO 527-1/-2
 10.2 MPa
@Strain 300 %
1480 psi
@Strain 300 %
200 mm/min; DIN 53504
Elongation at Break 528 %528 %200 mm/min; DIN 53504
Tensile Modulus  0.0290 GPa
@Temperature 60.0 °C
4.21 ksi
@Temperature 140 °F
storage; ISO 6721-1,-4
 0.0300 GPa
@Temperature 20.0 °C
4.35 ksi
@Temperature 68.0 °F
storage; ISO 6721-1,-4
 0.106 GPa
@Temperature -20.0 °C
15.4 ksi
@Temperature -4.00 °F
storage; ISO 6721-1,-4
Rebound 48 %48 %Resilience; ISO 4662
Tear Strength 45.0 kN/m257 pliISO 34-1
Abrasion 2525mm³, Method A; ISO 4649
Compression Set  22 %
@Temperature 23.0 °C
22 %
@Temperature 73.4 °F
72 hr; ISO 815
 25 %
@Temperature 70.0 °C
25 %
@Temperature 158 °F
24 h; ISO 815
 17 %
@Temperature 70.0 °C,
Time 86400 sec
17 %
@Temperature 158 °F,
Time 24.0 hour
Method C; ISO 815-1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 225 - 235 °C437 - 455 °FInjection
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °FInjection
Ejection Temperature 50.0 °C122 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmopan® 385 E Polyurethane
Covestro Desmopan® 5377A Polyurethane
Covestro Desmopan® 3385A Polyurethane
Covestro Desmopan® 3485A Polyurethane
Covestro Desmopan® 385 S Polyurethane

PB09763 / 92603

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.