MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay RHODOLINE® DF-988 Surfactant
Categories: Fluid

Material Notes: Description: Silicone free and mineral oil free defoamer for high gloss paints.

Identification: DEFOAMER

Available in: North America

Applications: RHODOLINE© DF-988 is a silicone-free, mineral oil-free and APE-free defoamer for use in waterborne coating formulations. Rhodoline DF-988 is especially designed to provide outstanding foam control in high sheen waterborne architectural formulation with no adverse effects on the coating gloss and create surface defects in coatings. Rhodoline DF-988 can also be used in semi gloss coatings adhesives and other waterborne formulations. Recommended usage levels are 0.1 – 0.5 % of defoamer as is based on total formulation

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.990 - 1.03 g/ccRP-17617
Viscosity 1500 - 2000 cPRP-0596
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceClear LiquidRP-0064

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay RHODOLINE® 622 Surfactant
Solvay RHODOLINE® 581B Surfactant
Solvay RHODOLINE® LC-2 Surfactant
Solvay RHODOLINE® WA-100 Surfactant
Solvay RHODOLINE® DF-665 Surfactant

WRHOD487 / 137718

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.