MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hostacom M3 U42 LW92607 Polypropylene with 30% Talc Filler  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Talc Filler

Material Notes: Hostacom M3 U42 LW92607 is a 30% talc filled PP homopolymer, with good detergent resistance and good color stability. Product is available as a customized color matched, pellet form. Product is UL listed. This grade is not intended for medical, pharmaceutical, food or drinking water applications. This grade is delivered in W92607 color version. Avoid prolonged storage in open sunlight. Storage at high temperatures (> 50°C) and high humidity may damage the packaging. Dry material before processing.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³
Melt Flow 17 g/10 min
@Load 2.16 kg,
Temperature 230 °C
17 g/10 min
@Load 4.76 lb,
Temperature 446 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 32.0 MPa4640 psi
Elongation at Break 3.5 %3.5 %
Elongation at Yield 3.5 %3.5 %
Tensile Modulus 3.30 GPa479 ksi
Flexural Modulus 3.40 GPa493 ksiTech.A
Charpy Impact Unnotched  1.60 J/cm²
@Temperature 0.000 °C
7.61 ft-lb/in²
@Temperature 32.0 °F
 2.60 J/cm²
@Temperature 23.0 °C
12.4 ft-lb/in²
@Temperature 73.4 °F
Charpy Impact, Notched 0.250 J/cm²
@Temperature 23.0 °C
1.19 ft-lb/in²
@Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °Funannealed
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Hostacom SP 98/F/94 1740 Polypropylene with 30% Talc Filler
LyondellBasell Hostacom M3 U42 LW92607 WHT Polypropylene with 30% Talc Filler
LyondellBasell Hostacom M3 N01 LW92607 WHT Polypropylene with 30% Talc Filler
LyondellBasell Hostacom HRC 183D G84014 Polypropylene with 30% Talc Filler
LyondellBasell Hostacom EKC 455P G82779 Polypropylene with 30% Talc Filler

PEQT8028 / 219664

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.