MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Baystar™ Lumicene® mPE M 3581 UV Metallocene Medium Density Polyethylene Rotational Molding Resin – Pellet Form
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Rotational Molded

Material Notes: Characteristics:
  • Second generation metallocene
  • Superior mechanical properties
  • Outstanding optical properties (gloss)
  • Improved dimensional stability
  • Easy processing
Applications:
  • NSF standard 51, 61
  • Rotational-molded items

This former Total Petrochemicals grade is now a part of the Bayport Polymers joint venture.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.935 g/ccASTM D-792
ESCR 100% Igepal® >= 1000 hourASTM D-1693
ESCR 10% Igepal® 300 hourASTM D-1693
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D-1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 1700 psiASTM D-638
Tensile Strength, Yield 2600 psiASTM D-638
Elongation at Break 340 %ASTM D-638
Elongation at Yield 8.0 %ASTM D-638
Tensile Modulus 93.0 ksiASTM D-638
Flexural Modulus 100 ksi
@Strain 1 %
Secant; ASTM D-790
Impact Test 180 ft-lb
@Thickness 6.35 mm
-40°C, ARM Low Temperature Impact
 
Thermal PropertiesOriginal ValueComments
Melting Point 252 °FASTM D-3417
Vicat Softening Point 239 °FASTM D-1525
 
Descriptive Properties
UV Rating16G155, cycle1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total Lumicene® mPE M 4041 UV Metallocene Polyethylene, Rotomolding
Total Lumicene® mPE M 4707 EP Metallocene Polyethylene, Blown Film
Total Lumicene® mPE M 5220 High Density Polyethylene, Blow Molding
Total Lumicene® MR10MX0 Metallocene Random Copolymer Polypropylene, Injection Molding and Injection Blow Molding
Total Lumicene® mPE M 3509 Medium Density Polyethylene, Blow Molding

PBAYST926 / 130502

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.