System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
SABIC LEXAN™ Copolymer FXM1414T Polycarbonate (PC) (Americas)
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
Material Notes:
PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.
Features: High Impact Resistance
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.18
g/cc
ASTM D792
Density
1.18
g/cc
ISO 1183
Moisture Absorption
0.0200 %
Injection Molding
0.0900 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation
0.12 %
ISO 62-1
Viscosity
9.0
cP
@Load 1.20 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow
0.0040
-
0.0080
cm/cm
SABIC method
0.0040
-
0.0080
cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse
0.0040
-
0.0080
cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow
10
g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
47.0
MPa
50 mm/min; ISO 527
48.0
MPa
50 mm/min; ASTM D638
Tensile Strength, Yield
56.0
MPa
50 mm/min; ISO 527
58.0
MPa
50 mm/min; ASTM D638
Elongation at Break
78 %
50 mm/min; ASTM D638
89 %
50 mm/min; ISO 527
Elongation at Yield
5.4 %
50 mm/min; ISO 527
5.7 %
50 mm/min; ASTM D638
Tensile Modulus
2260
MPa
50 mm/min; ASTM D638
2270
MPa
1 mm/min; ISO 527
Flexural Strength
85.0
MPa
yld, 1.3 mm/min, 50 mm span; ASTM D790
88.0
MPa
yield, 2 mm/min; ISO 178
Flexural Modulus
2120
MPa
2 mm/min; ISO 178
2230
MPa
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched
520
J
ASTM D256
270
J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO)
30.0
kJ/m²
80*10*4; ISO 180/1A
14.0
kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched
40.0
kJ/m²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy
57.0
J
ASTM D3763
Electrical Properties
Original Value
Comments
Comparative Tracking Index
175
-
250
V
UL 746A
Hot Wire Ignition, HWI
15
-
30
sec
@Thickness >=1.50 mm
UL 746A
High Amp Arc Ignition, HAI
60
-
120
arcs
@Thickness >=1.50 mm
UL 746A
>=
120
arcs
@Thickness >=3.00 mm
UL 746A
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
67.5
µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E831
67.5
µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow
80.0
µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E831
80.0
µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Hot Ball Pressure Test
75.0
°C
PASS; IEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi)
119
°C
Flatw 80*10*4 sp=64mm; ISO 75/Af
120
°C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point
138
°C
Rate B/50; ISO 306
139
°C
Rate B/50; ASTM D1525
142
°C
Rate B/120; ISO 306
UL RTI, Electrical
80.0
°C
UL 746B
UL RTI, Mechanical with Impact
80.0
°C
UL 746B
UL RTI, Mechanical without Impact
80.0
°C
UL 746B
Flammability, UL94
HB
@Thickness >=1.50 mm
UL 94
Glow Wire Ignition Temperature
825
°C
@Thickness 1.50 mm
IEC 60695-2-13
850
°C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index
800
°C
@Thickness 1.50 mm
IEC 60695-2-12
960
°C
@Thickness 3.00 mm
IEC 60695-2-12
Processing Properties
Original Value
Comments
Nozzle Temperature
290
-
310
°C
Zone 2
280
-
305
°C
Zone 3
295
-
315
°C
Melt Temperature
295
-
315
°C
Injection Molding
Mold Temperature
70.0
-
95.0
°C
Drying Temperature
120
°C
Injection Molding
Dry Time
3.00
-
4.00
hour
Injection Molding
48.0
hour
Cumulative; Injection Molding
Back Pressure
0.300
-
0.700
MPa
Shot Size
40 - 60 %
Vent Depth
0.00250
-
0.00760
cm
Screw Speed
40
-
70
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PSABH80291 / 288238
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.