MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient Elastamax™ HTE 3150 PVC+NBR  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Elastamax™ HTE Series thermoplastic elastomers (TPEs) are based upon compounded blends of PVC resins and nitrile rubber. These elastomeric materials provide outstanding resistance to hydrocarbons and oils, offer excellent weatherability, and are an economical alternative to thermoset rubber and other more costly thermoplastic elastomers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Melt Flow 42 g/10 min
@Load 5.00 kg,
Temperature 190 °C
Procedure A; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 52
@Time 15.0 sec
ASTM D2240
Tensile Strength at Break 11.9 MPaType IV, 510 mm/min; ASTM D638
Tensile Stress at Strain 2.91 MPa
@Strain 100 %
Type IV, 510 mm/min; ASTM D638
 7.34 MPa
@Strain 300 %
Type IV, 510 mm/min; ASTM D638
Elongation at Break 470 %Type IV, 510 mm/min; ASTM D638
Tear Strength 24.7 kN/mDie C, 510 mm/min; ASTM D624
Compression Set 49 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395A
 58 %
@Temperature 100 °C,
Time 79200 sec
ASTM D395A
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -55.0 °CASTM D746
 
Descriptive Properties
AppearanceBlack
FeaturesGeneral Purpose
FormsPellets
Generic NamePolyvinyl Chloride + NBR (PVC+NBR)
Processing MethodExtrusion
 Injection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAutomotive Applications
 Construction Applications
 General Purpose
 Industrial Applications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Armacell ArmaSport® AMC-Med Continuous Roll, PVC/NBR
Avient Elastamax™ HTE 3070 Polyvinyl Chloride + NBR (PVC+NBR)
Avient Elastamax™ HTE 3060 Polyvinyl Chloride + NBR (PVC+NBR)
Avient Elastamax™ HTE 3050 Polyvinyl Chloride + NBR (PVC+NBR)
Armacell Ensolite™ SF0 PVC/NBR

PH1PN8105 / 101941

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.