MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AISI Type M2 Molybdenum High Speed Tool Steel (UNS T11302)
Categories: Metal; Ferrous Metal; Tool Steel; Cold Work Steel

Material Notes: Used in high speed tool and cutting applications such as drills, milling processes, reamers, etc. Mo and W content promotes toughness and aids cutting properties, but requires more precise hardening conditions and caution about overheating. Quench via oil, air, or salt bath.

Composition for UNS T11302 covers both reg C and high C versions of AISI M2.

Data taken from the reference(s) and manufacturer data.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.14 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 61 - 64Austenitized and Tempered
 64 - 66Oil Quenched from between 1121°C to 1232°C
Modulus of Elasticity 207 GPa
Charpy Impact 23.0 - 28.0 ft-lbAustenitized and Tempered
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000540 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.5 µm/m-°C
@Temperature 20.0 - 100 °C
 11.7 µm/m-°C
@Temperature 20.0 - 200 °C
 12.2 µm/m-°C
@Temperature 20.0 - 300 °C
 12.4 µm/m-°C
@Temperature 20.0 - 400 °C
 12.7 µm/m-°C
@Temperature 20.0 - 500 °C
 12.9 µm/m-°C
@Temperature 20.0 - 700 °C
 13.0 µm/m-°C
@Temperature 20.0 - 600 °C
Specific Heat Capacity 0.460 J/g-°C
Thermal Conductivity 19.0 W/m-K
 
Processing PropertiesOriginal ValueComments
Processing Temperature 540 - 595 °CTempering
 1190 - 1230 °CHardening
Annealing Temperature 870 - 900 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.78 - 0.88 %AISI M2 reg C
 0.95 - 1.05 %AISI M2 high C
Chromium, Cr 3.75 - 4.5 %
Iron, Fe 78 - 82.4 %As Balance
Manganese, Mn 0.15 - 0.40 %
Molybdenum, Mo 4.5 - 5.5 %
Nickel, Ni <= 0.30 %
Silicon, Si 0.20 - 0.45 %
Tungsten, W 5.5 - 6.75 %
Vanadium, V 1.75 - 2.2 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type A2 Tool Steel
Crucible Steel Rex M2 High Speed Steel
AISI Type D2 Tool Steel, air quenched at 1010°C, tempered at 200°C
Carpenter Speed Star® High Speed Steel (Red-Hard) (AISI M2)
Bohler-Uddeholm UDDEHOLM VANADIS 30 AISI M2 + Co SUPERCLEAN 3 Powder Metallurgical Cold Work Tool Steel

MSTM2 / 178338

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.