MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ZEON HyTemp® SC-75 Polyacrylate Curative
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: HyTemp SC-75 is a 75% active dispersion of a proprietary cure system. The dispersion functions as a cure package in HyTemp 4050 series elastomers. This provides fast property development; excellent shelf stability and good scorch resistance. The dispersion is in the form of green pellets dusted with clay and free from foreign materials.

Fast cure package for HyTemp 4050 and 4060 series (75% active)

Key Words: ACM
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.01 g/cc1.01 g/cc
 
Component Elements PropertiesMetricEnglishComments
Nitrogen, N 3.4 - 4.8 %3.4 - 4.8 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Baytec® 505 Polyurethane
Chemours Viton® A-700 with 3 phr Curative and 6 phr Ca(OH)2
ATG s.r.l. EPDM Ethylene-Propylene Terpolymer
ZEON HyTemp® ZFC-65 Polyacrylate Curative
Monmouth Rubber & Plastics Durafoam™ P391SHD EPDM

PZEONC43 / 73102

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.