MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Unifrax IsoMat® AV5 Substrate Support Mat
Categories: Ceramic

Material Notes: IsoMat AV5 is designed to function as mechanical support for the ceramic substrate and act as an exhaust gas seal while providing thermal insulation.

IsoMat AV5 offers superior performance at low temperatures and has excellent thermal stability with a continuous use temperature of 750°C average mat temperature (Reference SAE Paper 2007-01-0471). Performance at low temperatures is provided by a structural support matrix of Isofrax® fibers held together by a proprietary binder system, and it is equivalent to typical non-intumescent support mat systems. At elevated temperatures, the fiber matrix support is complemented by vermiculite expansion to absorb additional gap expansion. As a result, the holding force of the system is maintained over a broad range of temperature. This makes IsoMat AV5 an ideal solution for a wide range of emission control devices, including large deisel oxidation catalysts (DOC), diesel particulate filters (DPF), and selective catalyst reduction units (SCR), as well as gasoline oxidation catalysts, including ethanol (flex fuel) underbody converters.

IsoMat AV5 has been designed to provide robust performance without the need for wire mesh ring protection (for erosion) or heat treatment for additional holding force at low temperatures.

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Loss On Ignition 2.5 - 7.5 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield >= 0.100 MPa
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.180 W/m-K
@Temperature 650 °C
ASTM C177
Maximum Service Temperature, Air 750 °C
 
Descriptive Properties
Isofrax® Fibers (%)65-75
Vermiculite (%)15-25

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CUNIF127 / 97899

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.