EMERGE™ PC 4310-22 advanced resin is high-performance polycarbonate resin offering high heat resistance, toughness, and superior flow. This resin is available in a full range of colors that can be custom tailored to meet your product requirements.
Applications: - Consumer Electronics and Information Technology Equipment
- Computer and Business Equipment
- Portable Electronics
Information provided by Dow |