MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Mobiltemp Series 1
Categories: Fluid; Lubricant; Clay Gellant; Polyalphaolefin (PAO)

Material Notes: Mobiltemp Series greases are high performance clay-thickened products designed for the lubrication of plain and antifriction bearings operating at low speed and high temperature or under cycling conditions from ambient to high temperatures. These greases use a clay thickener, which, unlike traditional soap thickeners, do not soften at high temperatures. They are based on a high quality, high viscosity mineral oil and are specially formulated to provide: low volatility and excellent resistance to oxidation at high temperatures, resistance to water washout and good anti-wear performance under heavy loads and low speeds. Mobiltemp 1 and 78 are NLGI Grade 1 greases, and Mobiltemp 2 is an NLGI 2 Grade. Mobiltemp 78 also contains molybdenum disulphide for added anti-wear protection. Mobiltemp Series greases are particularly suited for high temperature applications, and are very resistant to water or steam contamination. These greases have excellent resistance to changes in consistency under both high temperature and cyclic conditions of heating and cooling. Even with severe working under such conditions, they will not soften or harden significantly. Because they use low volatility base oils, these greases resist hardening when the grease is held at high temperatures for long periods. Mobiltemp Series greases have excellent resistance to water washing and, under humid conditions, can absorb about its own weight of water without any major change in structure or consistency. Mobiltemp Series have good flow properties and can be used with centralised grease systems down to 10ºC, even with long distribution lines. With its additional anti-wear additization, Mobiltemp 78 is particularly suitable for the lubrication of sliding machine elements subject to limited or slow motion or shock loading. With their excellent track record of superior performance in critical high temperature applications, Mobiltemp Series greases have become the products of choice for users around the world.

Mobiltemp 1 and Mobiltemp 2 are recommended for the lubrication of plain and antifriction bearings or sliding machine elements in applications operating at low speeds and high temperatures or under cycling conditions from ambient to high temperatures. The grease will not soften and leak under high temperature conditions or harden excessively on cooling. The recommended operating temperature range is 0 to 170º C, with even higher temperatures for short periods, with appropriate relubrication intervals. Mobiltemp 78 is recommended for similar applications to Mobiltemp 1 but the presence of molybdenum disulphide makes it particularly suitable for the lubrication of sliding machine elements subject to long relubrication intervals, limited motion or shock loading. The recommended operating temperature range is 0 to 170º C. Specific applications for Mobiltemp greases include: Oven conveyor chain bearings; Kiln car wheel bearings; Glass manufacture conveyer belt roller bearings; Cams, ways and other sliding machine elements (especially Mobiltemp 78)

Key Words: NLGI Grade 1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Kinematic Viscosity at 40°C (104°F) 460 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 31.7 cStASTM D445
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Load Wear Index 50ASTM D2596
Four Ball Extreme Pressure, Weld Load 200 kgASTM D2596
Four Ball Wear 0.500 mmASTM D2266
Penetration -60.0Penetration Change, Wet Roll Stability, 0.1 mm; ASTM D1831
 50Penetration Change, 60X to 100000X, mm/10; ASTM D217
 325Worked, 25°C; ASTM D217
 
Thermal PropertiesOriginal ValueComments
Dropping Point 300 °CASTM D2265
 
Descriptive Properties
Coloramber
Copper Strip Corrosion, ASTM D40481A
Soap/Thickener Typeclay

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WEXXON409 / 75834

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.